Hot stamping foil adhesion is measured in a number of different ways, and there is a lot of misconception about what each test really measures. Take the simple scratch test for example. Is that a definitive adhesion test or simply a measure of the hardness of one’s fingernail?

In fact, most adhesion tests carried out are comparative rather than a true measure. If you have two foils on the same substrate, both blocked at the same time, then you can test their comparative resistance to your fingernail, assuming that you do not subconsciously scratch harder on that you want to fail. This is more common than you might think, which is why a true scientific measure of adhesion is preferred.

However, such measurements are rare, and there is nothing that could realistically be routinely carried out by a trade blocker or printer. Even a rub or abrasion tester is not testing adhesion as much as the hardness of the foil surface. The so-called вЂ

About the Author

Author: Paul Norman | Total views: 230
Word Count: 668
Rating: Not yet rated | Votes: 0

Spanish taslation

For more information on hot stamping foil adhesion and other problems associated with their use, check out Paul’s website on Hot Stamping Foil that is designed to provide information the foil user, not sell products.




Rate, comment or bookmark this article

Seed Newsvine
Bookmark this article in your preferred program
AddThis Social Bookmark Button

Comments

No comments posted.

Add Comment

You do not have permission to comment. If you log in, you may be able to comment.

HTML code


use the code below to reprint this article on your website.


Creative Commons License
This article is licensed under a Creative Commons Attribution-Noncommercial-No Derivative Works 3.0 License.